Nanoindentation of Natural Materials
Spar

Nanoindentation of Natural Materials

innbundet, 2018
Engelsk

Nanoindentation of Natural Materials: Hierarchical and Functionally Graded Microstructures provides a systematic introduction and review of state-of-the-art statistical hierarchical and functionally graded structures found in bone, teeth, hair, and scales, from a nanoindentation perspective, including detailed microstructure and composition.

It covers the basics of hierarchical and functionally graded structures and nanoindentation techniques and detailed discussion with correlation micro/nano mechanical-structures

The book includes practical issues backed with experimental data

Undertittel
Hierarchical and Functionally Graded Microstructures
ISBN
9781498784054
Språk
Engelsk
Vekt
665 gram
Utgivelsesdato
24.9.2018
Antall sider
212