Residual Stresses and Nanoindentation Testing of Films and Coatings
This book covers the basic principles and application of nanoindentation technology to determine residual stresses in films and coatings. Subsequently, nanoindentation is used to determine residual stresses in different types of films and coatings, and to describe them in detail.