Fractography of Glasses and Ceramics V
Spara

Fractography of Glasses and Ceramics V

inbunden, 2007
Engelska
This volume contains papers presented at The Fifth Conference on the Fractography of Glasses and Ceramics Held in Rochester, New York, July 9-13 2006. Chapters include The Fracture Process at the Crack Tip, Fundamental Phenomena, Fractography of Contact Damage in Glasses and Ceramics, Identifying and Understanding Flaws in Ceramics, Fractography of Dental and Biomaterials, Fractography of Components, and Fracture Phenomena in Geology. This text provides a useful one-stop resource for understanding the most important issues in the research and applications of fractography of glasses and ceramics.